Place the chips in a boron furnace (note the white boron chips) to P-dope the exposed surfaces.  Nitrogen should flow at $1 ft^3/hr$ for 30 minutes at $950^oC$.

Place the chips in a boron furnace (note the white boron chips) to P-dope the exposed surfaces. Nitrogen should flow at $1 ft^3/hr$ for 30 minutes at $950^oC$.