aph9-lab3-04

The chips are loaded into an oxide furnace at $1000^o C$ for 40 minutes (the first 30 minutes are oxygen; the last 10 are nitrogen - to anneal the chips).

The chips are loaded into an oxide furnace at $1000^o C$ for 40 minutes (the first 30 minutes are oxygen; the last 10 are nitrogen – to anneal the chips).